• White Epoxy Primer Automotive Primer Paint Dry Grinding Corrosion Resistant
  • White Epoxy Primer Automotive Primer Paint Dry Grinding Corrosion Resistant
White Epoxy Primer Automotive Primer Paint Dry Grinding Corrosion Resistant

White Epoxy Primer Automotive Primer Paint Dry Grinding Corrosion Resistant

Product Details:

Place of Origin: China
Brand Name: ShangFu
Model Number: TGM-407

Payment & Shipping Terms:

Minimum Order Quantity: ≥300 Liters
Price: Negotiation
Packaging Details: 4L + 1L set, 3 sets and 1 ctn
Delivery Time: 10-25 days from the date of order confirmation
Payment Terms: Visa, Paypal, T/T, Western Union, MoneyGram
Supply Ability: 20000 Cartons Monthly production
Get Best Price Contact Now

Detail Information

Other Name: Automobile Primer Color: Grey,white,black,red
Application Method: Spray Service: OEM Or ODM
Characteristic: Excellent Corrosion Protection, Excellent Adhesion On The Surface Of Steel, Aluminum And Zinc Plates Usage: Car Paint, Appliance Paint, Boat Paint, Plastic Coating, Building Coating
Adaptive Environment: No Fire Source, Use In A Well Ventilated Environment Shelf Life: 2 Years In Original Sealed Can At Cool And Dry Place At 20℃
High Light:

automotive epoxy paint

,

automotive undercoat paint

Product Description

 

Automotive primer paint dry grinding white epoxy primer 2k car primer preventing corrosion rust resistant paint

 

 

Product Description:
A primer for preventing corrosion of metals,stronger adhesion ordinary epoxy primer, improve the anti-corrosion performance
 
It is used for the metal primer of all kinds of light corrosion, the steel structure of the road and bridge, vehicle, machine, the pipe surface and other light corrosion environment.
 
 
Epoxy primer
Code-name Product name Specification packing specifications Application and characteristics
TGM-407 White epoxy primer 4L+1L 3sets/piece A primer for preventing corrosion of metals
TGM-408 Grey epoxy primer 4L+1L 3sets/piece
TGM-409  High quality epoxy primer 4L+1L 3sets/piece Stronger adhesion than ordinary epoxy primer, improve the anti-corrosion performance
 
 
Epoxy primer
Applicable surface Original coating aluminum, steel, stainless steel, zinc steel zinc surface, polyester board, plywood, atomic ash
Volatilization time the interval between two layers is 5-10 minutes
Mix proportion tgm-408 epoxy primer:4
Special curing agent for grey epoxy primer:1
Epoxy thinner:1.5-2.0
Service life 20 ℃ 5 hours; 28 ℃ 4 hours;If the drying time exceeds 48 hours at 20 ℃, the iron red epoxy primer must be polished before spraying again
Spraying equipment and air pressure Gravity gun 1.2-1.5 mm 2-4 kg/cm Suction gun 1.4-1.8mm 3-5kg/cm
Spray 2-3 single coats
Temperature 10 ℃ 20 ℃   60 ℃
Non stick time 60 minutes 15 minutes   5 minutes
Drying time before grinding 16 hours 12 hours   50 minutes
Polish Before spraying: p80 dry grinding or wet grinding After spraying: p280-p380 dry grinding or p400-p800 wet grinding

 

 

Construction technology:

1. Clean&Shade

Remove wax oil and other impuritieswith deoiling detergent Examine andassess the location and extent of damage.

 

2. Grind damaged parts

Grinding with abrasive paper(#80# 2000). Dry grinding withsandpaper(#80, 120, 180) first.

 

3. Dust cleaning

Use a degreaser to remove greasefrom the workpiece.

 

4. Fill& Grind

Add thne hardener I proportionmix and fill the putty, Sanding(#80. 120, 180) after drying.

 

5. Clean &Grind

Clean the surface again, and thenfinely grind the filling to the leveof the paint.

 

6. Spray primer surfacer

Mix and spray primer according toproduct requirements, each layerneeds to be matte.

 

7. Grind primer surfacer

After the primer is dried, dry sandingpaper(3320-400)is used with atwo-way sander. Manual grindingon the edge(#600-800)

 

8. Clean & Wipe

Use a cleaner to clean the grease.and tack cloth to clear of dustand particles.

 

9. Spray 1K color paint

Add thinner as requiredspray2-3ayers, spray interval of 5-10nutes per layer.

 

10. Spray Varnish(clear coat)

Add hardener and thinner asrequired, spray two layerseach interval is 5-10 minutes.

 

11. Dry Bake

After the varnish is sprayed. it needbe allowed to stand for 10-15minutes can be baked or driednatur.

 

12. Waxing &Polish

Can be sanded with abrasivepaper(#2000)first if necessaryThen use related products forwaxing and polishing

 

 

Saft Precautions :

1. Keep container in a well ventilated and cool place

2. Keep away from fire

3. Avoid contact with eye and skin

4. Wear suitable gloves and eyes protection

5. Don't empty into drains

6. Against static discharges

Want to Know more details about this product
I am interested in White Epoxy Primer Automotive Primer Paint Dry Grinding Corrosion Resistant could you send me more details such as type, size, quantity, material, etc.
Thanks!
Waiting for your reply.